certainPL Low Temperature Aluminum Welding Rod No Need Solder Powder, 20"(1.6mm) (10Pcs)
Sold Out / Out of Stock
This item may be available in a different size, colour, scent, version or platform:
certainPL Low Temperature Aluminum Welding Rod No Need Solder Powder, 20"(1.6mm) (10Pcs)
Recommended for Welding or Brazing Aluminum Alloy - 1060, 1350, 3003, 3004, 3005, 5005, 5050, 6053, 6061, 6951, 7005, and cast alloys 710.0 and 711.0.
Great Welding Effect - With full & smooth welding effect because of internal powder. With low melting point(647℃~658℃), great weldability and corrosion resistance, high thermal conductivity, high electric conductivity and excellent processing performance.
Widely Application - It is mainly used for argon arc welding and filling material for pure aluminum, connection with aluminium bus and guide rod of electrolytic aluminium plant and electric power, chemistry, food and so on.
No Need Solder Powder - You don't have to use other flux powder with aluminum alloy as the welding core and coating as the salt base. Very convenient and easy to weld.
Widely Use In Life - Suitable for welding or surfacing welding alloy with high strength, good forgeability & good corrosion resistance.
Storage: placed in a ventilated and dry place, can be stored for a long time
 Size:50X0.16cm
 Quantity: 10/20/50PCS
  Material: Aluminum
 Color: Silver
 Melting Point: 647℃~658℃
 Diameter: 1.6mm / 0.062"
 Length: 500mm / 19.7"
 Recommended for welding or brazing aluminum alloy: 1060, 1350, 3003, 3004, 3005, 5005, 5050, 6053, 6061, 6951, 7005, and cast alloys 710.0 and 711.0
 Item Wight: Approx. 2.5g
 How to Use:
 Step 1: Clean and polishe the physical surface.
 Step 2: Heat the surface of the base material, until the temperature of the wire to the operating temperature of 380℃~400℃, so you can rely on the parent metal heat transfer welding wire to form welds, should not use the flame to burn wire.
 Step 3: When repairing thin aluminum, as long as the aluminum base metal heated to the appropriate working temperature, and then use the wire back and forth friction melting to form a weld, only with a metal brush melt welding wire to weld at the weld.
 Step 4: Use propane gas to weld s mall object, natural slow cooling after welding.
 NOTE:
 1. The surface of the base metal must be clean.
 2. The base metal temperature to reach 400 degrees, including the process of welding the base metal temperature should be maintained at 400℃, and the temperature can be high or low